I-Cuni44yi-alloy ye-copper-nickel (i-Cu56Ni44 alloy) ephawulwa kukumelana okuphezulu kombane, ukuguguleka okuphezulu kunye nokumelana okuhle kokugqwala. Ifanelekile ukusetyenziswa kumaqondo obushushu afikelela kwi-400°C
Iindlela eziqhelekileyo zokusetyenziswa kweCuNi44 zii-potentiometers ezizinzileyo kubushushu, ii-rheostats zemizi-mveliso, ii-electric motor starter resistances kunye ne-strain gauge.
Ukudibanisa i-coefficient yobushushu obungenamsebenzi kunye ne-resistivity ephezulu kwenza i-alloy ifaneleke ngokukodwa ekujijeni kwe-resistors ezichanekileyo.
I-CuNi44 yenziwe nge-electrolytic copper kunye ne-nickel ecocekileyo. Ngobukhulu obuncinci beengcingo, i-alloy ibizwa ngokuba yi-I-Cuni45(I-Thermocouple).
Ingcaciso yeMveliso
IConstantan ikwalilungu elingalunganga le-thermocouple yohlobo lwe-J apho i-Iron iyinto elungileyo; ii-thermocouple zohlobo lwe-J zisetyenziswa kwiindlela zokunyanga ubushushu. Kwakhona, lilungu elingalunganga le-thermocouple yohlobo lwe-T ene-OFHC Copper elilungileyo; ii-thermocouple zohlobo lwe-T zisetyenziswa kumaqondo obushushu aphantsi.
Umxholo weeKhemikhali, %
| Ni | Mn | Fe | Si | Cu | Okunye | Isikhokelo seROHS | |||
| Cd | Pb | Hg | Cr | ||||||
| 44 | 1.50% | 0.5 | - | I-Bal | - | ND | ND | ND | ND |
Iipropati zoomatshini
| Ubushushu beNkonzo eQhubekayo obuphezulu | 400ºC |
| Ukuqina kwakhona kwi-20ºC | 0.49±5%ohm mm2/m |
| Uxinano | 8.9 g/cm3 |
| Ukuqhuba kweThermal | -6(Ubuninzi) |
| Indawo yokunyibilika | 1280ºC |
| Amandla okuThamba, i-N/mm2 eqhotyoshelweyo, ethambileyo | 340~535 Mpa |
| Amandla okuThamba, i-N/mm3 eQokelelweyo ebandayo | 680~1070 Mpa |
| Ukwandiswa (i-anneal) | 25% (Ubuncinane) |
| Ukwandiswa (okuqengqelekayo okubandayo) | ≥Mncinci)2% (Mncinci) |
| I-EMF vs i-Cu, μV/ºC (0~100ºC) | -43 |
| Ulwakhiwo lweMicrographic | i-austenite |
| Ipropati yeMagnetic | Hayi |