Ukwakhiwa kweekhemikhali
ukwakhiwa | C | P | S | Mn | Si |
≤ | |||||
Umxholo (%) | I-0.03 | I-0.02 | I-0.02 | 0.6 ~ 1.1 | I-0.3 ~ 0.5 |
ukwakhiwa | Ni | Cr | Mo | Cu | Fe |
Umxholo (%) | I-49.0 ~ 51.0 | - | - | I-0.2 | I-bal |
Iipropathi zomzimba
Uphawu lwevenkile | Ukwanda kwe-Commar | Ukuxhathisa (μm) | Ukuxinana (G / CM³) | I-curie point (ºc) | I-Watnetostricturesty |
1J50 | 9.20 | I-0.45 | 8.2 | I-500 | 25.0 |
Inkqubo yonyango lobushushu
uphawu lwevenkile | Iphakathi | ubushushu bokufudumeza | Gcina ixesha lobushushu / h | Inqanaba lokupholisa |
1J50 | I-hydrogen yomile okanye i-vacuum, uxinzelelo alukho ngaphezulu kwe-0.1 pa | Kunye ne-tiace yokufumana i-1100 ~ 1150ºc | I-3 ~ 6 | Kwi-100 ~ 200 ºc / h ukupholisa ukuya kwi-600 ºc, ngokukhawuleza ukuya kwi-300 ºc Zoba intlawulo |