Wamkelekile kwiiwebhusayithi zethu!

Uns K93600 Invar 36 Ribbon Precision Expansion Alloy Wire Flat

Inkcazelo emfutshane:


  • Isicelo:Inqwelomoya, i-Electronics, iShishini, uNyango, imichiza
  • Umgangatho:JIS, GB, DIN, BS, ASTM, AISI
  • Ubunyulu:36%Ni
  • Ingxubevange:Ingxubevange
  • Uhlobo:Fe Ni Strip
  • Umgubo:Hayi Powder
  • INOMBOLO yoMfanekiso.FeNi36
  • Umphezulu:Igudile kwaye iBright
  • I-OEM:Ewe
  • Ipakethe yezoThutho:Ityala lomthi
  • Imvelaphi:eTshayina
  • Izinto:Fe- Ni Alloy
  • Umqathango:Ithambile
  • Sebenzisa:Izinto Zokutywina
  • Uphawu lwentengiso:TANKII
  • Inkcazo:0.1-8mm
  • Ikhowudi ye-HS:7505120000
  • Iinkcukacha zeMveliso

    FAQ

    Iithegi zeMveliso

    Uns K93600 Invar36 Ribhoni Precision Ukwandiswa kweAlloy Wire Flat

    (Igama eliqhelekileyo: Invar, FeNi36, Invar Standard, Vacodil36)

    4J36 (Invar), eyaziwa ngokubanzi njenge-FeNi36 (i-64FeNi e-US), i-alloy ye-nickel-iron ephawulekayo ngenxa ye-coefficient ephantsi yokwandiswa kwe-thermal (CTE okanye α).

    I-4J36 (I-Invar) isetyenziswa apho uzinzo oluphezulu olufunekayo, olufana nezixhobo ezichanekileyo, iiwotshi, iigeyiji ze-seismic creep, iifreyimu zesithunzi sesithunzi sikamabonakude, iivalvu kwiimotor, kunye newotshi ye-antimagnetic. Ekuhlolweni komhlaba, xa i-oda yokuqala (i-high-precision) yokunyusa umgangatho kufuneka yenziwe, abasebenzi beNqanaba (intonga yokulinganisa) esetyenzisiweyo yenziwe nge-Invar, endaweni yomthi, i-fiberglass, okanye ezinye izinyithi. I-Invar struts isetyenziswe kwezinye iipiston ukukhawulela ukwanda kwe-thermal ngaphakathi kweesilinda zazo.

    I-4J36 isebenzisa i-oxyacetylene welding, i-arc ye-arc yombane, i-welding kunye nezinye iindlela ze-welding. Ekubeni i-coefficient yokwandisa kunye nokwakheka kweekhemikhali ze-alloy inxulumene kufuneka igwenywe ngenxa ye-welding ebangela utshintsho kwi-alloy composition, kungcono ukusebenzisa i-Argon arc welding filler metals ekhethwayo iqulethe i-0.5% ukuya kwi-1.5% titanium, ukwenzela ukuba ukunciphisa i-weld porosity kunye nokuqhekeka.

    Ukwakheka okuqhelekileyo%

    Ni 35~37.0 Fe UBhal. Co - Si ≤0.3
    Mo - Cu - Cr - Mn 0.2~0.6
    C ≤0.05 P ≤0.02 S ≤0.02

    I-Coefficient yokwandiswa

    θ/ºC α1/10-6ºC-1 θ/ºC α1/10-6ºC-1
    20~-60 1.8 20-250 3.6
    20~-40 1.8 20-300 5.2
    20~-20 1.6 20~350 6.5
    20~-0 1.6 20-400 7.8
    20~50 1.1 20-450 8.9
    20-100 1.4 20~500 9.7
    20-150 1.9 20~550 10.4
    20-200 2.5 20-600 11.0

     

    Iimpawu ezibonakalayo eziqhelekileyo

    Ubuninzi (g/cm3) 8.1
    Ukumelana nombane kwi-20ºC(OMmm2/m) 0.78
    Iqondo lobushushu le-resistivity(20ºC~200ºC)X10-6/ºC 3.7~3.9
    I-Thermal conductivity, λ/ W/(m*ºC) 11
    Indawo yeCurie Tc/ ºC 230
    Imodyuli yeElastic, E/Gpa 144

     

    Inkqubo yonyango lokushisa
    I-Anealing yokunciphisa uxinzelelo Ukufudumala ukuya ku-530 ~ 550ºC kwaye ubambe i-1 ~ 2 h. Kuyabanda
    ukuhlamba Ukuze kupheliswe ukuqina, okuveliswe kwinkqubo yokuzoba epholileyo, ebandayo. I-Annealing ifuna ukufudunyezwa kwi-830 ~ 880ºC kwi-vacuum, bamba i-30 min.
    Inkqubo yozinziso
    1. Kwimidiya ekhuselayo kwaye ishushu kwi-830 ºC, bamba i-20min. ~ 1h, cima
    2. Ngenxa yoxinzelelo olwenziwa ngokucinywa, ukufudumala ukuya kwi-315ºC, bamba i-1 ~ 4h.
    Ukulumkela
    1. Ayinakuqiniswa ngonyango lobushushu
    2. Ukunyangwa komphezulu kunokuqhunyiswa kwesanti, ukupolisha okanye ukuchola.
    3. Ingxubevange ingasetyenziswa 25% hydrochloric acid pickling isisombululo kwi 70 ºC ukucima umphezulu oxidized.

    Iimpawu zoomatshini eziqhelekileyo

    Tensile strength Ukwandisa
    Mpa %
    641 14
    689 9
    731 8

    Iqondo lobushushu lokumelana

    Uluhlu lobushushu, ºC 20~50 20-100 20-200 20-300 20-400
    aR/ 103 *ºC 1.8 1.7 1.4 1.2 1.0

  • Ngaphambili: