I-Ni35Cr20 yi-alloy ye-nickel-chromium (i-alloy ye-NiCr) ephawulwa yi-resistivity ephezulu, ukumelana okuhle kwe-oxidation, uzinzo oluhle kakhulu kwimo, i-ductility elungileyo kunye ne-weldability egqwesileyo. Ifanelekile ukusetyenziswa kumaqondo obushushu afikelela kwi-1100°C.
Ukusetyenziswa okuqhelekileyo kwe-OhmAlloy104A kusetyenziswa kwizifudumezi zokugcina ebusuku, kwizifudumezi ze-convection, kwizifudumezi ze-rheostats ezinzima kunye nezifudumezi zefeni. Kwaye ikwasetyenziswa kwiintambo zokufudumeza kunye nezifudumezi zentambo kwizinto zokunyibilikisa nokususa i-icing, iingubo zombane kunye nee-pad, izihlalo zeemoto, izifudumezi zebhodi yesiseko kunye nezifudumezi zomgangatho, izithinteli.
Ulwakhiwo oluqhelekileyo%
| C | P | S | Mn | Si | Cr | Ni | Al | Fe | Okunye |
| Ubuninzi | |||||||||
| 0.08 | 0.02 | 0.015 | 1.00 | 1.0~3.0 | 18.0~21.0 | 34.0~37.0 | - | Ibhala. | - |
Iimpawu eziqhelekileyo zeMechanical (1.0mm)
| Unikeze Amandla | Tensile strength | Ukwandiswa |
| I-Mpa | I-Mpa | % |
| 340 | 675 | 35 |
Iimpawu eziqhelekileyo zomzimba
| Ubuninzi (g/cm3) | 7.9 |
| Ukumelana kombane kwi-20ºC(Ωmm2/m) | 1.04 |
| I-coefficient yokuqhuba kwi-20ºC (WmK) | 13 |
| I-coefficient yokwandiswa kobushushu | |
| Ubushushu | I-Coefficient yoKwandiswa koBushushu x10-6/ºC |
| 20 ºC- 1000ºC | 19 |
| Umthamo othile wobushushu | |
| Ubushushu | 20ºC |
| I-J/gK | 0.50 |
| Iqondo lokunyibilika (ºC) | 1390 |
| Ubushushu obuphezulu bokusebenza obuqhubekayo emoyeni (ºC) | 1100 |
| Iimpawu zeMagnetic | okungekho magnethi |
Izinto Ezichaphazela Ubushushu Bokumelana Nombane
| 20ºC | 100ºC | 200ºC | 300ºC | 400ºC | 500ºC | 600ºC |
| 1 | 1.029 | 1.061 | 1.09 | 1.115 | 1.139 | 1.157 |
| 700ºC | 800ºC | 900ºC | 1000ºC | 1100ºC | 1200ºC | 1300ºC |
| 1.173 | 1.188 | 1.208 | 1.219 | 1.228 | - | - |