I-CRAL 205 yintsimbi ye-iron-chromium-aluminium alloy (i-FeCrAl alloy) ebonakaliswe ngokuchasa okuphezulu, i-coefficient ephantsi yokumelana nombane, ubushushu obuphezulu bokusebenza, ukumelana nokugqwesa kakuhle phantsi kweqondo lokushisa eliphezulu.Kufanelekile ukusetyenziswa kwiqondo lokushisa ukuya kwi-1300 ° C.
Usetyenziso oluqhelekileyo lwe-CRAL 205 lusetyenziswa kwiziko lombane loshishino, i-cooktop ye-ceramic yombane.
Ukwakheka okuqhelekileyo%
| C | P | S | Mn | Si | Cr | Ni | Al | Fe | Okunye |
| Max | |||||||||
| 0.04 | 0.02 | 0.015 | 0.50 | Ubuninzi 0.4 | 20.0-21.0 | Ubuninzi 0.10 | 4.8-6 | UBhal. | / |
Iimpawu ezibonakalayo eziqhelekileyo
| Ubuninzi (g/cm3) | 7.10 |
| Ukumelana nombane kwi-20℃(ohmm2/m) | 1.39 |
| I-coefficient yokuqhuba kwi-20℃ (WmK) | 13 |
| Amandla Okuqina (Mpa) | 637-784 |
| Ukwandisa | Ubuncinci 16% |
| Ukubopha(HB) | 200-260 |
| ICandelo lokwahluka kweRate yokucutha | 65-75% |
| Ukugoba ngokuphindaphindiweyo | Min 5 amaxesha |
| I-Coefficient yokwandiswa kwe-thermal | |
| Ubushushu | I-Coefficient yoKwandiswa kweThermal x10-6/℃ |
| 20 ℃- 1000℃ | 16 |
| Umthamo wobushushu obuthile | |
| Ubushushu | 20℃ |
| J/gK | 0.49 |
| Indawo yokunyibilika (℃) | 1500 |
| Ubushushu obuphezulu obuqhubelekayo bokusebenza emoyeni (℃) | 1300 |
| Iimpawu zemagneti | kazibuthe |