I-Constantan Konstantan CuNi44Mn1 i-Copper Nickel wire 0.6mm yeengcingo zokufudumeza.
I-Tankii Alloys i-alloy ye-copper - i-nickel (i-CuNi44Mn1 i-alloy) ebonakaliswe ngokuxhatshazwa kombane ophezulu, i-ductility ephezulu kunye nokuchasana nokugqwesa okulungileyo. Ilungele ukusetyenziswa kumaqondo obushushu ukuya kuma-400°C. Usetyenziso oluqhelekileyo lwe-Tankii Alloys bubushushu - ii-potentiometers ezizinzileyo, ii-rheostats zamashishini kunye nokuchasana kwe-motor starter yombane.
Ukudityaniswa kwe-coefficient yobushushu obungakhathaliyo kunye nokumelana okuphezulu kwenza i-alloy ilungele ngokukhethekileyo ukugoba kwezichasi ezichanekileyo.
I-alloys yenziwe kwi-electrolytic copper kunye ne-nickel ecocekileyo yi-Tankii Co.Ltd, i-alloy ikhethwe kwaye ifumaneka kwiisayizi ezininzi zeengcingo.
Ukwakheka okuqhelekileyo%
Isiqalelo | Umxholo |
---|---|
Nickel | 45 |
IManganese | 1 |
Ubhedu | UBhal. |
Iipropati zoomatshini eziqhelekileyo (1.0mm)
Ipropati | Ixabiso |
---|---|
Amandla esivuno (Mpa) | 250 |
Amandla Okuqina (Mpa) | 420 |
Ubude (%) | 25 |
Iimpawu ezibonakalayo eziqhelekileyo
Ipropati | Ixabiso |
---|---|
Ubuninzi (g/cm3) | 8.9 |
Ukumelana nombane kwi-20℃ (Ωmm²/m) | 0.49 |
Iqondo lobushushu lokumelana (20℃~600℃)X10⁻⁵/℃ | -6 |
I-coefficient yokuqhuba kwi-20℃ (WmK) | 23 |
EMF vs Cu(μV/℃ )(0~100℃ ) | -43 |
I-Coefficient yokwandiswa kwe-thermal
Uluhlu lobushushu | Ukwandiswa kweThermal x10⁻⁶/K |
---|---|
20 ℃ – 400℃ | 15 |
Umthamo wobushushu obuthile
Ubushushu | Ixabiso (J/gK) |
---|---|
20℃ | 0.41 |
Indawo yokunyibilika (℃)|1280|
|Ubushushu obuqhubekayo bokusebenza emoyeni (℃)|400|
|Iimpawu zemagneti|ezingezozibuthe|
I-alloys-Ukusebenza kokusingqongileyo okuSebenzayo
Igama lengxubevange | Ukusebenza emoyeni kwi-20℃ | Ukusebenza kubushushu obuphezulu 200℃ (Umoya kunye neoksijini ziqulethe iigesi) | Ukusebenza kubushushu obuphezulu 200℃ (iigesi ezineNitrogen) | Ukusebenza kubushushu obuphezulu 200 ℃ (iigesi ezinesulfure - oxidability) | Ukusebenza kubushushu obuphezulu 200 ℃ (iigesi ezinesulfure - ukuncitshiswa) | Ukusebenza kwiqondo lobushushu eliphezulu 200℃ (carburization) |
---|---|---|---|---|---|---|
Tankii Alloys | kulungile | kulungile | kulungile | kulungile | embi | kulungile |
Isimbo soNikezo
Igama le-alloys | Uhlobo | Ubungakanani |
---|---|---|
Tankii Alloys-W | Ucingo | D = 0.02mm ~ 1mm |
Tankii Alloys-R | Iribhoni | W = 0.4 ~ 40, T = 0.03 ~ 2.9mm |
Tankii Alloys-S | Ukuhluba | W = 8 ~ 200mm, T = 0.1 ~ 3.0 |
Tankii Alloys-F | I-Foil | W = 6 ~ 120mm, T = 0.003 ~ 0.1 |
Tankii Alloys-B | Ibha | Dia = 8 ~ 100mm, L = 50 ~ 1000 |