Umxholo weeKhemikhali, %
| Ni | Mn | Fe | Si | Cu | Okunye | Isikhokelo seROHS | |||
| Cd | Pb | Hg | Cr | ||||||
| 44 | 1.50% | 0.5 | - | I-Bal | - | ND | ND | ND | ND |
Iipropati zoomatshini
| Ubushushu beNkonzo eQhubekayo obuphezulu | 400ºC |
| Ukuqina kwakhona kwi-20ºC | 0.49±5%ohm mm2/m |
| Uxinano | 8.9 g/cm3 |
| Ukuqhuba kweThermal | -6(Ubuninzi) |
| Indawo yokunyibilika | 1280ºC |
| Amandla okuThamba, i-N/mm2 eqhotyoshelweyo, ethambileyo | 340~535 Mpa |
| Amandla okuThamba, i-N/mm3 eQokelelweyo ebandayo | 680~1070 Mpa |
| Ukwandiswa (i-anneal) | 25% (Ubuncinane) |
| Ukwandiswa (okuqengqelekayo okubandayo) | ≥Mncinci)2% (Mncinci) |
| I-EMF vs i-Cu, μV/ºC (0~100ºC) | -43 |
| Ulwakhiwo lweMicrographic | i-austenite |
| Ipropati yeMagnetic | Hayi |